| Availability: | |
|---|---|
din93
The washer body must support the fastener and remain sufficiently flat during tightening and tab forming.
The tab must withstand controlled plastic deformation into the specified lock position.
The transition radius r influences local strain where the tab joins the washer body. It must conform to the approved geometry.
Burrs, sheared-edge cracks or coating defects can initiate failure during bending.
Steel is a documented DIN 93 category. One Fastenal plain-product specification requires steel with a light protective oil finish for its own product standard.
For steel supply, specify:
grade and condition;
formability requirement;
hardness limit if relevant;
thickness tolerance;
surface condition;
coating system;
material certificate.
Do not apply bolt property classes to the washer unless a washer-specific specification explicitly requires them.
A2 is commercially documented for DIN 93 washers. It may be evaluated for corrosion resistance and clean appearance, but exact grade, temper and bendability require supplier confirmation.
A4 variants are also commercially documented. They may be considered for more demanding corrosion environments, subject to application-specific review and availability.
Fasteners.eu lists brass as a non-ferrous commercial category. Brass performance, strength, work hardening and environmental compatibility must be validated separately.
Potential DIN 93 supply conditions include:
plain/lightly oiled steel;
zinc-coated steel;
natural or passivated stainless condition;
another specified treatment subject to supplier capability.
The washer's bright appearance in the uploaded image does not prove zinc plating or stainless steel.
Tab installation produces plastic deformation that may:
crack a brittle coating;
expose base metal;
cause flaking;
damage passivation;
create local corrosion sites;
change cosmetic appearance.
A coating qualified on an unbent washer may not remain intact after forming. Where corrosion matters, inspect or test the bent condition.
Plain or lightly protected steel may be considered where humidity and corrosion risk are low, subject to maintenance.
Specify a defined coating or suitable stainless category, including corrosion-test requirements.
A4 stainless may be evaluated, but no material is universally immune to crevice or galvanic corrosion.
Review galvanic compatibility among the washer, fastener, housing and reaction feature.
Temperature can affect material ductility, coatings and corrosion. No service-temperature range is provided by DIN 93 dimensions.
Select material and finish only after reviewing the actual chemical environment.
Material selection must maintain the specified:
inside diameter d1;
outside diameter d2;
tab width b;
axis-to-tab-end distance l;
thickness s;
transition radius r.
The DIN-authorised reference table spans M3–M52. Thickness varies from 0.38 mm in small sizes to 1.6 mm in larger sizes, affecting forming tools and bend behaviour.
Thread |
|
|
|
|
|
|
|---|---|---|---|---|---|---|
M3 | 3.2 | 12 | 4 | 13 | 0.38 | 2.5 |
M4 | 4.3 | 14 | 5 | 14 | 0.38 | 2.5 |
M8 | 8.4 | 22 | 8 | 20 | 0.75 | 4 |
M12 | 13.0 | 30 | 12 | 28 | 1.00 | 10 |
M24 | 25.0 | 50 | 20 | 42 | 1.00 | 10 |
M27 | 28.0 | 58 | 23 | 48 | 1.60 | 16 |
M39 | 40.0 | 82 | 32 | 64 | 1.60 | 16 |
M52 | 54.0 | 105 | 44 | 85 | 1.60 | 16 |
Values are millimetres and come from the Fasten.it DIN-authorised table, cross-checked with Fasteners.eu.
verify material and coating documents;
inspect tab edges and root radius;
avoid scratching the washer during positioning;
tighten the fastener before final tab forming;
use smooth tools with controlled contact surfaces;
bend without creating sharp nicks;
inspect for cracks and coating failure;
apply an approved repair treatment if specified;
document bent-condition acceptance.
Requirement | Buyer input |
|---|---|
Material | Steel, A2, A4, brass or specified grade |
Grade/standard | Exact designation |
Condition/temper | Formability requirement |
Thickness | DIN size or approved drawing |
Surface treatment | Exact process |
Coating thickness | Value and test method |
Corrosion test | Method, duration and acceptance |
Bend test | Angle/tooling and pass criteria |
Coating-after-bend | Crack/flaking limits |
Certificates | Material, finish and compliance records |
material identification;
thickness measurement;
hardness/formability checks where specified;
dimensional inspection;
burr and edge inspection;
coating-thickness testing;
bend testing;
post-bend crack inspection;
corrosion testing in formed condition where required;
lot traceability.
A2/A4 availability varies by size and supplier.
Stainless labels do not by themselves define temper or bendability.
Zinc coatings may crack during forming.
Brass is not automatically suitable for high-load assemblies.
No universal corrosion-life value is provided.
Material cannot be inferred from the photograph.
Reuse after straightening is not automatically acceptable.
Reference directories list steel, A2 stainless, A4 stainless and brass categories.
No. It is a commercial finish option. Plain/lightly oiled steel and stainless variants also exist.
The silver-grey appearance is insufficient to identify the material.
The forming operation can crack or expose the coating at the tab bend.
Bendability depends on grade, temper, thickness and tooling. Validate the actual supplied material.
Provide size, grade, condition, finish, corrosion environment, bending method, coating-after-bend criteria, quantity, certificates and packaging.